Pocket-spring mattresses
An EVA for pocket-spring mattress assembly, with a short-to-medium open time.
- Viscosity 160 °C
- 2,200–2,400 mPa·s
- Softening point
- 103–110 °C
- Application
- 140–170 °C
Different assemblies, one question: what open time, viscosity and adhesion does the job need?
EVA · polyolefin · sprayable · nozzle-applied
An EVA for pocket-spring mattress assembly, with a short-to-medium open time.
EVA grades for carpet fringe and rug assembly, plus general assembly work.
A high-viscosity EVA for anti-slip back coating on carpets and rugs.
A polyolefin with a long open time for laminating and coating textiles.
Anti-scratch hot melts for ceramic tiles, in EVA and polyolefin.
| Family | Viscosity 160 °C, mPa·s | Softening point, °C | Application, °C | Compliance | Typical use |
|---|---|---|---|---|---|
| EVA | 550–6,000 | 98–118 | 140–200 | — | Mattresses, carpets, tile protection |
| Polyolefin | 1,500–6,000 | 105–120 | 140–180 | — | Textile lamination, tile protection |
Carpet back-coating grade: 9,000–11,000 mPa·s at 200 °C. Bands span the grades we supply in each family. Figures are a starting point for sampling; the current TDS and CoA govern.
Packed in 20–25 kg bags.
Technical and safety data sheets, a certificate of analysis on every lot, and the declarations your quality team will ask for — sent without you having to chase them. Figures shown on this site are a starting point for sampling; the current TDS and CoA govern.
An EVA at around 2,200–2,400 mPa·s at 160 °C, with a short-to-medium open time.
Yes — a high-viscosity EVA for anti-slip back coating.
Yes, in EVA and polyolefin.
Tell us the substrates, line speed and service conditions. We will tell you straight whether we have a grade for it.
A line or two about what you are making is enough to start — we’ll take it from there.